Publication database
Laser micro-machining is a rapidly growing technique to create, manufacture and fabricate microstructures on different materials ranging from metals and ceramics to polymers. Micro- and nano-machining on different materials has been helpful and useful for various biomedical applications. This study focuses on the micro-machining of innovative barbed sutures using an ultrashort pulse laser, specifically a femtosecond (fs) laser system. Two bioresorbable polymeric materials, namely, catgut and poly (4-hydroxybutyrate) (P4HB), were studied and micro-machined using the femtosecond (fs) laser system. The optimized laser parameter was used to fabricate two different barb geometries, namely, straight and curved barbs. The mechanical properties were evaluated via tensile testing, and the anchoring performance was studied by means of a suture–tissue pull-out protocol using porcine dermis tissue which was harvested from the medial dorsal site. Along with the evaluation of the mechanical and anchoring properties, the thermal characteristics and degradation profiles were assessed and compared against mechanically cut barbed sutures using a flat blade. The mechanical properties of laser-fabricated barbed sutures were significantly improved when compared to the mechanical properties of the traditionally/mechanically cut barbed sutures, while there was not any significant difference in the anchoring properties of the barbed sutures fabricated through either of the fabrication techniques. Based on the differential scanning calorimetry (DSC) results for thermal transitions, there was no major impact on the inherent material properties due to the laser treatment. This was also observed in the degradation results, where both the mechanically cut and laser-fabricated barbed sutures exhibited similar profiles throughout the evaluation time period. It was concluded that switching the fabrication technique from mechanical cutting to laser fabrication would be beneficial in producing a more reproducible and consistent barb geometry with more precision and accuracy.
Femtosecond laser processing combines highly accurate structuring with low residual heating of materials, low thermal damage, and nonlinear absorption processes, making it suitable for the machining of transparent brittle materials. However, with high average powers and laser pulse repetition rates, residual heating becomes relevant. Here, we present a study of the femtosecond laser pulse-on-demand operation regime, combined with regular scanners, aiming to improve throughput and quality of processing regardless of the scanner’s capabilities. We developed two methods to define the needed pulse-on-demand trigger sequences that compensate for the initial accelerating scanner movements. The effects of pulse-on-demand operation were studied in detail using direct process monitoring with a fast thermal camera and indirect process monitoring with optical and topographical surface imaging of final structures, both showing clear advantages of pulse-on-demand operation in precision, thermal effects, and structure shape control. The ability to compensate for irregular scanner movement is the basis for simplified, cheaper, and faster femtosecond laser processing of brittle and heat-susceptible materials.
Experimental investigation into ultrashort laser ablation by burst and Single Pulse (SP) modes on Polypropylene was performed. Isolated craters with different set of laser parameters were produced on flat polymer samples to assess the influence of the temporal separation between pulses on surface quality, removal rate (time needed to remove a certain volume) and ablation efficiency (pulse energy needed to remove a certain volume). The laser parameters that allow the development of structures with minimum redeposited material splashed around them and maximum removal rates were identified. Pulse energies of 2.5 μJ and 6 μJ were identified as the removal pulse energy threshold and the value from which a structure depth saturation starts, respectively.
The use of bursts provides improved quality and higher removal rates compared to the Single Pulse mode when the same number of pulses of identical pulse energies were emitted in both cases, even though the total eliminated volume is higher in the SP mode. The advantages of using bursts of 3 pulses are reported. Increasing the number of pulses per burst to 4 do not increase the removal rate when compared to bursts of 3 pulses.